Uniaxial Hot Press (HP) - Goliath Stein Heurtey Physitherm
  • 0.01 mbars
  • Max. Temp. 2100°C
  • Max. Press. 100 kN
  • Vac/Ar/N2

Synthesis Chemical/Materials > Materials > Press > HP Sintering

This hot press allows densification of powders (ceramic, metallic, composites) under high pressure. Thermal treatments can be performed too. Pressures applied are high uniaxial pressures. Several atmospheres (Vaccum; Ar; N2) are possible. The maximum temperature is 2100°C with an heating rate of 25°C/min. The volum chamber is Ø140x190 mm. Existing several cylincal mold with a diameter of 10, 19, 25, 37 and 50mm. You can contact the platform manager to more information.

Contact Task Facility Manager (TFM)

0472437929

Depending structure

MATEIS

345 Avenue Gaston Berger
69100 Villeurbanne
+33(0)4 72 43 83 82

infos : Website

Other's Laboratory/Plateforme

Email


Laboratory : Plateforme de Frittage

Sandrine Cottrino Dankic

Responsable Plateforme Frittage

Depending structure : MATEIS
Federation :

ICL|INGELYSE|CLYM|METSA


Lab tutorship :

UCBL, CNRS, INSA


7 Avenue Jean Capelle

69100 Villeurbanne

Full support :
Continuous education :
Access with light support :
Open to academic :
Open to enterprises :

MEANS.FR

Powered by

Newsletter

Register to Fabrique de l'innovation newsletter

Copyright © 2022 Means. Tous droits réservés.
internet conception